MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nurel Engineering Polymers Promyde® B30 U PA 6, Conditioned, UL certified, Flame retardant, Heat stabilized, Nucleated and Lubricated  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized; Nylon 6, Nucleated; Nylon 6, Unreinforced, Flame Retardant

Material Notes: Characteristics: Promyde B30 U is an improved flame retardant polyamide 6, UL certified, heat stabilized, lubricated and nucleated for fast cycle injection molding. Its main characteristics are easy flowing, easy mould filling and very fast cooling time whilst maintaining excellent polyamide 6 mechanical properties.

Applications: Due to its improved Glow Wire Flammability Index of 960ºC, easy flow characteristics and very fast cooling time; Promyde B30 U is suitable for multi cavity and single cavity injection molding of flame resistant parts such as components used in automotive, electrical, electronics, or technical parts.

Information provided by Nurel Engineering Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Moisture Absorption 3.00 %50%, rh; ISO 62
Water Absorption at Saturation 9.5 %in water; ISO 62
Viscosity Test 145 cm³/gViscosity Number; ISO 307
Linear Mold Shrinkage, Flow 0.0090 - 0.011 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 - 0.011 cm/cm
Melt Flow 145 g/10 min
@Load 5.00 kg,
Temperature 275 °C
[cm3/10 min], MVR; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 40.0 MPa50 mm/min; ISO 527-1/-2
Elongation at Break >= 50 %50 mm/min; ISO 527-1/-2
Elongation at Yield 25 %50 mm/min; ISO 527-1/-2
Tensile Modulus 1100 MPa1 mm/min; ISO 527-1/-2
Flexural Strength 30.0 MPa2 mm/min; ISO 178
Flexural Modulus 1000 MPa2 mm/min; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 30.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Dielectric Constant 7.0
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CDSC 10°C/min; ISO 3146
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °Cinjection molding
Mold Temperature 40.0 - 80.0 °C
Drying Temperature <= 80.0 °C
Dry Time 4.00 - 6.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNUREL008 / 183373

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.