MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Colorite Polymers 8088 Non-Phthalate 88 Series Vinyl Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doorway applications, as well as inside refrigerated area separators. In both cases, low temperatures are likely to be encountered. All components that are used in the manufacturing of these compounds are sanctioned by the U.S. Food and Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulation. Also, because they sanctioned by the US Department of Agriculture, they may be used in meat packaging plants and other food handling areas with no risk of contamination from the entry separators.

Information provided by Colorite Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength, Ultimate 2600 psiASTM D638
Elongation at Break 350 %ASTM D638
100% Modulus 1.25 ksi
@Strain 100 %
ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -52.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Colorite Polymers 7588 Non-Phthalate 88 Series Vinyl Compound
Colorite Polymers 8011G-015 (Extrustion), 8012G-015 (Molding) Radiation Sterilizable Vinyl Compound
Colorite Polymers 9088 Non-Phthalate 88 Series Vinyl Compound
Colorite Polymers 2010 Rigid PVC
Colorite Polymers 8077 Non-Phthalate 77 Series Vinyl Compound

PCOL132 / 28851

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.