MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nylene® Nylene 494P BLK Specialty Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Specially formulated nylon powder for the ROTOMOLDING process. Heat stabilized. Dried to less than 0.20% moisture and packaged in foil-lined drums to eliminate the need for pre-drying. Strongly recommend the use of an inert gas such as nitrogen in the mold to minimize thermal degradation during processing.

Testing conducted on dry as molded specimen at 73°F

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Viscosity Measurement 7070Relative Viscosity; ASTM D789
Linear Mold Shrinkage 0.015 - 0.020 cm/cm0.015 - 0.020 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 79.0 MPa11500 psiASTM D638
Elongation at Break 70 %70 %ASTM D638
Flexural Modulus 2.552 GPa370.1 ksiASTM D790
Izod Impact, Notched 0.480 J/cm0.899 ft-lb/inASTM D256
Dart Drop, Total Energy  27.1 J
@Thickness 3.56 mm,
Temperature -40.0 °C
20.0 ft-lb
@Thickness 0.140 in,
Temperature -40.0 °F
ARM
 38.0 J
@Thickness 3.56 mm,
Temperature -20.0 °C
28.0 ft-lb
@Thickness 0.140 in,
Temperature -4.00 °F
ARM
 108 J
@Thickness 3.56 mm,
Temperature 23.0 °C
80.0 ft-lb
@Thickness 0.140 in,
Temperature 73.4 °F
ARM
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 180 °C356 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNYLEN982 / 221514

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.