MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Engineered Syntactic Systems SF-32 Subsea Syntactic Void Filler
Categories: Polymer; Thermoset; Epoxy

Material Notes: SF-32 is a specially engineered syntactic formulated to serve as a void filler for subsea applications. The material is provided as a three-part kit that is mixed and poured into any free-flood cavity or void. The mix is allowed to cure at room temperature to form a solid syntactic material that will withstand repeated ocean excursions to depths of 3,000 feet. The easily cast system is provided in three parts; two resin components and a solid filler. The two resin components are mixed together, followed by the glass bubble filler. When the three materials are uniformly mixed, the moderate viscosity combination may be poured into its desired location. Initial cure will occur over a twenty four hour period at ambient temperatures, (50°F - 90 °F), providing a solid, lightweight article which is ready for any secondary operation such as machining, finishing or painting. Full cure will take place after 7 – 10 days. The cured material will provide an average of 32 pounds of buoyancy per cubic foot in seawater.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 32.0 lb/ft³
Water Absorption <= 3.0 %
@Time 86400 sec
at 3000 ft.depth
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 2400 psi
Compressive Modulus >= 160 ksi
Hydrostatic Design Basis 2900 psiHydrostatic Crush Strength (6600 feet)
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Monthfrom manufacture date
 
Descriptive Properties
ColorWhite/Tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Engineered Syntactic Systems SF-38 Subsea Syntactic Void Filler
Engineered Syntactic Systems SF-30 Subsea Syntactic Void Filler
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding

PESS963 / 93185

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.