MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sharadaa Ceramics Smart Cast 9 Medium Cement Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.35 g/ccAfter Drying at 110°C
Grain Size <= 10000 µm
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00000157 GPa
@Temperature 110 °C
 0.00000167 GPa
@Temperature 1100 °C
 0.00000196 GPa
@Temperature 1500 °C
Compressive Strength 1250 kg(f)/cm²
@Temperature 110 °C
Cold Crushing
 1550 kg(f)/cm²
@Temperature 1100 °C
Cold Crushing
 1600 kg(f)/cm²
@Temperature 1500 °C
Cold Crushing
 300 kg(f)/cm²
@Time 86400 sec
Cold Crushing
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.49 W/m-K
@Temperature 400 °C,
Time 10800 sec
 1.63 W/m-K
@Temperature 800 °C,
Time 10800 sec
Maximum Service Temperature, Air 1500 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 >= 50 %
Fe2O3 <= 1.1 %
 
Descriptive Properties
Permanent Linear Change-0.1 - 0.1%800
 -0.2 - 0.2%1100
 -0.2 - 0.2%1500
Thermal Expansion0.5Reversible
Water Required to Mix4-5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CSHARA124 / 130287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.