MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 1095 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 25 mm (1 in.) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; High Carbon Steel

Material Notes: Applications include edge tools, wear-resistant parts, high-stress flat springs, hot coiled springs, plow beams, plow shares, scraper blades, discs, mower knives, and harrow teeth. Post oil quenched hardness: 46 HRC surface, 42 HRC half-radius, 40 HRC center

Key Words: UNS G10950, AMS 5121, AMS 5122, AMS 5132, AMS 7304, ASTM A29, ASTM A510, ASTM A576, ASTM A682, FED QQ-S-700 (C1095), MIL SPEC MIL-S-16788 (C10), SAE J403, SAE J412, SAE J414, DIN 1.1274, JIS SUP 4, SS14 1870 (Sweden), B.S. 060 A 96, B.S. EN 44 B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/ccTypical for steel.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 321
Hardness, Knoop 348Converted from Brinell
Hardness, Rockwell B 99Converted from Brinell
Hardness, Rockwell C 35Converted from Brinell
Hardness, Vickers 339Converted from Brinell
Tensile Strength, Ultimate 1105 MPa
Tensile Strength, Yield 655 MPa
Elongation at Break 13.2 %in 50 mm
Reduction of Area 32.4 %
Modulus of Elasticity 200 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel.
Poissons Ratio 0.29Typical For Steel
Shear Modulus 80.0 GPaTypical for steel.
Izod Impact 3.00 Jannealed at 790°C (1450°F)
 4.00 Jas rolled
 5.00 Jnormalized at 900°C (1650°F)
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000180 ohm-cm
@Temperature 20.0 °C
condition of specimen unknown
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 0.000 - 100 °C
 11.7 µm/m-°C
@Temperature 0.000 - 200 °C
 12.4 µm/m-°C
@Temperature 0.000 - 300 °C
 13.1 µm/m-°C
@Temperature 0.000 - 400 °C
 13.5 µm/m-°C
@Temperature 0.000 - 500 °C
 14.2 µm/m-°C
@Temperature 0.000 - 600 °C
 14.6 µm/m-°C
@Temperature 0.000 - 700 °C
Specific Heat Capacity 0.461 J/g-°C
@Temperature >=100 °C
Thermal Conductivity 51.9 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.90 - 1.03 %
Iron, Fe 98.38 - 98.8 %As remainder
Manganese, Mn 0.30 - 0.50 %
Phosphorus, P <= 0.040 %
Sulfur, S <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1095 Steel, oil quenched 800°C (1470°F), 480°C (900°F) temper, 25 mm (1 in.) round
AISI 1095 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 1095 Steel, normalized at 900°C (1650°F), air cooled, 25 mm (1 in.) round
AISI 1095 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1095 Steel, oil quenched from 800°C (1475°F), tempered at 480°C (900°F)

M1095R / 7117

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.