MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Rilsan® Fine Powders T WHITE 1488 AC PA11
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Powder

Material Notes:

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccCoating; ISO 1183
Bulk Density 0.500 g/cc0.0181 lb/in³Fluidized
 0.550 g/cc0.0199 lb/in³Non Tapped; ISO 1068
 0.660 g/cc0.0238 lb/in³Tapped; ISO 1068
Water Absorption <= 1.0 %
@Time 86400 sec
<= 1.0 %
@Time 24.0 hour
ISO 62-1
Particle Size 100 - 130 µm100 - 130 µmMedian; ISO 13320
Thickness <= 250 microns<= 9.84 milRecommended Coating Thickness
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ISO 868
Impact Test >= 2.00 J>= 1.48 ft-lbImpact Resistance; ASTM G14
Taber Abrasion, mg/1000 Cycles 1313Wheel CS 17, load 1 kg; ISO 9352
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 kV/mm
@Thickness 0.350 - 0.450 mm
762 kV/in
@Thickness 0.0138 - 0.0177 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
Melting Point 183 - 188 °C361 - 370 °FISO 1218
Vicat Softening Point 181 °C358 °FISO 306
 
Descriptive Properties
Approximate RAL number9010
ColorWhite
Covering Efficiency (kg/m²)0.35
Covering Efficiency, Thickness (µm)300
Form as DeliveredPowder
Grade Package Weight - Bags (lb/bag)55
Moisture SensitiveNo
Persoz Hardness240ISO 1522
Salt Spray TestGood adhesion after 2000 hoursISO 9227 (surface preparation per ARKEMA)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARKF622 / 291300

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.