MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mo-Sci Corporation GL-0175 Barium-Titanate Glass Spheres
Categories: Ceramic; Glass; Oxide; Titanium Oxide

Material Notes: Appearance: Solid glass microspheres with light yellow color in powder form.

Typical applications of GL0175 beads include:: high temperature spacer material for gauge control, coating, filler for plastic, retroreflection applications and etc.

Information provided by Mo-Sci Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.80 g/ccof Dry Beads
Density 4.20 - 4.50 g/cc
pH 7.0in water
 
Thermal PropertiesOriginal ValueComments
Softening Point 600 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.90
 
Component Elements PropertiesOriginal ValueComments
B2O3 1.0 - 20 %
BaO 40 - 70 %
SiO2 1.0 - 20 %
TiO2 40 - 70 %
ZrO2 1.0 - 10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Elements Barium Titanate nanoparticles
Barium Titanate, BaTiO3
Harris Acoustic Sensors EC-21 Barium Titanate Piezoelectric
Mateck Barium Titanate Crystal, BaTiO3
Channel Industries 300 Barium Titanate Piezoelectric

CMOSCI012 / 137195

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.