MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A.D. Compound Adene NCTAG Copolymer 50% CaCO3 Filled Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Information provided by A.D. Compound

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Filler Content 50 %50 %ISO 3451 / 1
Melt Index of Compound 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ISO 868
Tensile Strength, Yield 16.0 MPa2320 psiISO 527
Elongation at Break 40 %40 %ISO 527
Elongation at Yield 6.0 %6.0 %ISO 527
Flexural Modulus 2.00 GPa290 ksiISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²8.57 ft-lb/in²ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C133 °FISO 75
Vicat Softening Point 78.0 °C172 °F49 N; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sinvicomp SRF 1807 Polyvinyl Chloride, Rigid
Karina 18/387-RG-GE (CS) Gray Color Concentrate for PVC
Colorite Polymers 9904 Clear Extrusion Vinyl Compound
BASF Elastollan® R 2002 25% Glass Filled TPUR
Aurora Plastics GA-1046CTLF PVC

PADCOM14 / 22592

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.