MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Autoclaved aerated concrete, 0.700 g/cc density
Categories: Ceramic; Concrete

Material Notes: Uniform cellular product made from a siliceous material (sand and/or pulverized-fuel ash) and cement or cement and lime. Cellular structure is produced usually by the incorporation of fine aluminum powder into the mix. Aerated concrete undergoes plastic deformation, or creep, under sustained loading. 100 mm wall of autoclaved concrete blocks, without surface finishing, has a fire resistance grading of 2 hours if load bearing, or 4 hours if non-load bearing. Easily sawn and drilled with hand tools. Vapor resistance of 60 MNs/gm. Applications include building blocks, reinforcing units, precast lintels, infill blocks for concrete floor and roof systems.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.700 g/cc
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.00 J/g-°C
Thermal Conductivity 0.210 W/m-K3% moisture content
 0.230 W/m-K5% moisture content

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Autoclaved aerated concrete, 0.600 g/cc density
Autoclaved aerated concrete, 2.100 g/cc density
Autoclaved aerated concrete, 0.750 g/cc density
Autoclaved aerated concrete, 0.900 g/cc density
Autoclaved aerated concrete, 0.800 g/cc density

CAA1C / 387

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.