MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cossa Polimeri ESTAPROP 1006 V2 K Flame Retardant Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Flame Retardant

Material Notes: PP copolymer

Flame retardant class V2, PBDE and antimony trioxide free, no blooming, low smoke emission, good physical and mechanical characteristics

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D 792
Linear Mold Shrinkage 0.015 - 0.018 cm/cmASTM D 955
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 28.0 MPaASTM D 638
Elongation at Break 100 %ASTM D 638
Flexural Modulus 1400 MPaASTM D 790
Izod Impact, Notched 40.0 J/m
@Temperature -20.0 °C
ASTM D 638
 50.0 J/m
@Temperature 0.000 °C
ASTM D 638
 60.0 J/m
@Temperature 23.0 °C
ASTM D 256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C120°C/hr; ASTM D 648
Vicat Softening Point 150 °C
@Load 0.999 kg
50°C/hr; ASTM D 1525
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
Glow Wire Test 960 °C
@Thickness 2.00 mm
I.E.C. 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 199 X 137777 C Polypropylene (PP) Copolymer - High Flow - High Impact - Flame Retardant - UV Stabilized
Avient Trilliant™ HC HC5220-0040 RS Natural Polypropylene
Overview of materials for Polypropylene Copolymer
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized
RTP Company RTP 150 HF Polypropylene (PP), High Flow - Unreinforced - Flame Retardant - UL94 V-0

PCOSSA873 / 156463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.