Description: K-430p is an expandable polystyrene grade containing pentane as a blowing agent. The product is delivered in the form of spherical beads with a bulk density of about 0.6 g/cm3 and is available in 1100 kg octabins. Applications: The properties of K-430p make it suitable for the production of light insulation boards by block moulding or special packaging applications. It suits particularly well for applications where low water uptake is needed, like frost insulation of building perimeter. Information provided by BEWi Synbra |