MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Delrin Delrin® 100 NC010 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: High Viscosity Acetal Homopolymer

Information provided by DuPont; Delrin was sold by DuPont in 2023.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccISO 1183
Melt Density 1.19 g/cc
@Temperature 215 °C
Water Absorption 0.27 %
@Time 86400 sec
Immersion; Sim. to ISO 62
 0.90 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cmISO 294-4, 2577
 0.030 cm/cmannealed; ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cmISO 294-4, 2577
 0.024 cm/cmannealed; ISO 294-4
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
cm³/10min Volumetric; ISO 1133
 2.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ISO 2039-2
Hardness, Rockwell R 121ISO 2039-2
Ball Indentation Hardness 173 MPaH 358/30; ISO 2039-1
Tensile Strength, Yield 71.0 MPaISO 527-1/-2
Elongation at Break 45 %Nominal; ISO 527-1/-2
Elongation at Yield 26 %ISO 527-1/-2
Tensile Modulus 2900 MPaISO 527-1/-2
Flexural Strength 93.0 MPaISO 178
 77.0 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 2800 MPaISO 178
Compressive Strength 110 MPa
@Temperature 204 °C,
Time 252000 sec
ISO 604
Poissons Ratio 0.37
Izod Impact, Notched (ISO) 13.0 kJ/m²
@Temperature -40.0 °C
ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 425 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2900 MPa1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 1600 MPa1000h; ISO 899-1
Abrasion 4.0mm3; DS; ISO 4649
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 3.00e+13 ohmIEC 62631-3-2
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 62631-2-1
 3.9
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 41.0 kV/mmIEC 60243-1
Dissipation Factor 0.0010
@Frequency 100 Hz
IEC 62631-2-1
 0.0055
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°CISO 11359-1/-2
 100 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°CISO 11359-1/-2
 100 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
Specific Heat Capacity 3.00 J/g-°C
@Temperature 215 °C
Melt
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 110 °CTemperature index, Tensile strength 20,000h; IEC 60216-1
 125 °CTemperature index, Tensile strength 5000h; IEC 60216-1
Deflection Temperature at 0.46 MPa (66 psi) 160 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CISO 75-1/-2
 115 °CAnnealed; ISO 75-1/-2
Vicat Softening Point 160 °C50°C/h, 50N; ISO 306
 175 °C50°C/h 10N; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
IEC 60695-11-10
 HB
@Thickness 1.50 mm
IEC 60695-11-10
Flame Spread 40.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Glow Wire Ignition Temperature 550 °C
@Thickness 0.400 mm
IEC 60695-2-12
 550 °C
@Thickness 0.750 mm
IEC 60695-2-13
 550 °C
@Thickness 1.00 mm
IEC 60695-2-13
 550 °C
@Thickness 1.50 mm
IEC 60695-2-13
 550 °C
@Thickness 2.00 mm
IEC 60695-2-13
 550 °C
@Thickness 3.00 mm
IEC 60695-2-13
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 °COptimum, Extrusion
 195 - 205 °CRange, Extrusion
 210 - 220 °CRange, Injection
 215 °COptimum, Injection
Mold Temperature 90.0 °COptimum, Injection
 80.0 - 100 °CInjection
Drying Temperature 80.0 °CInjection
 80.0 °CExtrusion
Dry Time 2.00 - 4.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Extrusion
 <= 0.20 %Injection
Hold Pressure 90.0 - 110 MPaInjection
 110 MPaInjection
Annealing Temperature 160 °COptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)1E-07
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0.1G-value (condensate); ISO 6452
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>POM<ISO 11469
PolymerPOM
Processing Hold Pressure Time (s/mm)8Injection
Resin IdentificationPOMISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 100 BK602 POM
Delrin Delrin® 100AL NC010 POM-S
Delrin Delrin® 150 NC010 POM
Delrin Delrin® 100P NC010 POM
Delrin Delrin® 100AF POM-PTFE20

PDSX5081 / 197721

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.