MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ 725 General Purpose Hot Melt Adhesive
Categories: Polymer; Adhesive

Material Notes: A clear general purpose hot melt adhesive great for many craft and product assembly projects. (65 second open time). This hot melt adhesive works well with both high and low temperature glue guns and a medium set time. It is a great all purpose hot melt adhesive and works well with both porous and non-porous materials.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Viscosity 4400 cP
@Temperature 191 °C
 9200 cP
@Temperature 163 °C
 33400 cP
@Temperature 121 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 126 °FPeel Adhesion Failure. ASTM D4498, 45# Kraft paper substrates, 500 g weights.
Flash Point >= 450 °F
Shear Adhesion Failure Temperature 161 °F45# Kraft paper substrates, 500 g weights.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 - 380 °FApplication
 
Descriptive Properties
Chemical CompositionEthylene Vinyl Acetate
Colorclear
Mettler Softening Point176°F, ASTM D6493-99
Odorslight
Open Time65 sec. ASTM D4497-94(1999), using 45# Kraft paper substrates

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Northern White Pine Wood
Overview of materials for Epoxy Adhesive, Flexible
Master Bond MB514 Hot Melt Adhesive Compound
Dow 722 Low Density Polyethylene (LDPE)

PCHEMI926 / 232181

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.