MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Carmel Olefins Capilene® CE 85 B Polypropylene, Extrusion Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: CAPILENE® CE 85 B is a specialty polypropylene combining typical advantages of polypropylene random and heterophasic copolymers, and is designed for extrusion applications. Features: Excellent impact, Very low stress whitening, Good organoleptic properties, Excellent transparency, High gloss, Short cycle time, Clarified, Mold release. Uses: Detergent and cosmetics, clear containers, High clarity films, Corrugated sheets, Profiles. Processing Methods: Blow Molding, Sheet extrusion, Thermoforming.

Information provided by Carmel Olefins Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 446 °F
1133
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 0.800 GPa116 ksi5mm/min; ISO 178
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
ISO 180
 20.0 kJ/m²
@Temperature 0.000 °C
9.52 ft-lb/in²
@Temperature 32.0 °F
ISO 180
 35.0 kJ/m²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C165 °FISO 75-2
Vicat Softening Point 131 °C
@Load 1.02 kg
268 °F
@Load 2.25 lb
ISO 306
 
Optical PropertiesMetricEnglishComments
Haze  3.0 %
@Thickness 0.0500 mm
3.0 %
@Thickness 0.00197 in
film; ASTM D1003
 10 %
@Thickness 1.00 mm
10 %
@Thickness 0.0394 in
plaque; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCARM814 / 249034

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.