MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wacker Powersil® 466 A/B Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® 466 A/B is a liquid silicone rubber with medium conductivity, stable electrical properties and good mechanical properties.

Special features:

    high elongation at break, low tension set
  • stable electrical properties
  • good mechanical properties
  • ready-to-use, two-component system
Application: POWERSIL® 466 A/B is suitable for production of electrically conductive injection molded articles, especially cable accessories in the medium and high voltage range. The range of use spreads from push-on accessories to cold shrink applications. POWERSIL® 466 A/B combines a low Shore A Durometer with high elongation, good setting properties (low tension set) and good mechanical properties which are a must for cold shrink applications.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183-1 A
Viscosity  550000 cP
@Shear Rate 10.0 1/s
550000 cP
@Shear Rate 10.0 1/s
Component B; ISO 3219
 600000 cP
@Shear Rate 10.0 1/s
600000 cP
@Shear Rate 10.0 1/s
Mix; ISO 3219
 650000 cP
@Shear Rate 10.0 1/s
650000 cP
@Shear Rate 10.0 1/s
Component A; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3838ISO 868
Tensile Strength at Break 7.00 MPa1020 psiISO 37
Elongation at Break 650 %650 %ISO 37
Tear Strength 28.0 kN/m160 pliASTM 624 B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 30 ohm-cm30 ohm-cmIEC 60093
 30 ohm-cm30 ohm-cmASTM D991
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
post-cured for 4h at 200°C
Pot Life 4320 min4320 min
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9371 / 204900

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.