MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Sodium Hydrogen Carbonate, NaHCO3 (Sodium Bicarbonate)
Categories: Ceramic

Material Notes: CAS Number: 144-55-8

Physical Form: White Monoclinic Crystals

Key Words: baking soda, bicarbonate of soda, sodium acid carbonate, NaHCO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.20 g/cc
Solubility in Water 10.3 %
Molecular Weight 84.007 g/mol
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.043 J/g-°CCrystal
Heat of Formation -950.8 kJ/molCrystal
Decomposition Temperature 50.0 °C
 
Descriptive Properties
SolubilitySoluble in H2O; Insoluble in EtOH

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Hydroxide, Gibbsite, Al(OH)3
DIAB Klegecell® R 260 Rigid, Closed Cell PVC Foam Core Material
Crystex Composites Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite
Röhm CYROLITE G-20 Acrylic-Based Multipolymer Molding Compound
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded

EINOR3157 / 5252

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.