MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled
Categories: Metal; Electronic/Magnetic Alloy; Superalloy; Iron Base

Material Notes: High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC circuits in which the frequency is less than 400 cycles per second. Following a low temperature hydrogen anneal at 1300/1400°F (704/760°C), alloy 49 exhibits constant permeability characteristics. Its initial permeability is approximately 500 Gauss. High Permeability "49" alloy resists weather and moisture corrosion to a moderate extent.

High permeability "49" alloy has been used in laminated cores for instrument transformers, magnetic shields and cores for certain electronic and communications devices in which extremely high permeability at low magnetizing forces greatly increases the efficiency and effectiveness of the equipment. Because of its high permeability, it has also been used in solenoid cores in light, sensitive relays that must operate and respond to weak currents that induce low magnetizing forces.

If components are to machined in volume from bar stock, High Permeability "49"-FM, a free-machining grade, is recommended. The standard grade , High Permeability "49" alloy, machines somewhat like the austenitic stainless alloys. It develops gummy chips but does not work harden as rapidly as the stainless alloys. Sulfur-bearing cutting compounds are highly detrimental to the final magnetic properties. Animal lard oil should be used in drilling and machining operations which must be performed at low speeds. Work hardened bars offer the best machining characteristics. Parts should be degreased and cleaned as soon as possible.

Information provided by High Temp Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 8.18 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 100
Tensile Strength, Ultimate 130000 psi
Elongation at Break 5.0 %
Modulus of Elasticity 166 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000480 ohm-cmTemperature coefficient = 0.0036/°C (-17.8 to 499°C)
Magnetic Permeability 8000
@Thickness 0.635 - 3.17 mm
Initial; B100; heat treatment unknown; ASTM A596
 12000
@Thickness 0.356 mm
Initial; B100; heat treatment unknown; ASTM A596
 <= 90000
@Thickness 0.635 - 3.17 mm
Maximum; heat treatment unknown; ASTM A596
 <= 150000
@Thickness 0.356 mm
Maximum; heat treatment unknown; ASTM A596
Magnetic Coercive Force, Hc 0.040 - 0.070 Oe
@Thickness 0.635 - 3.17 mm
from 10,000 Gauss; heat treatment unknown; ASTM A596
 0.040 - 0.070 Oe
@Thickness 0.356 mm
from 10,000 Gauss; heat treatment unknown; ASTM A596
Magnetic Saturation Flux Density, Bmax 15000 Gauss
@Thickness 0.356 mm
H-100 Oersted; after hydrogen annealing; ASTM A596
 15000 Gauss
@Thickness 0.635 - 3.17 mm
H-100 Oersted; after hydrogen annealing; ASTM A596
Magnetic Remanence, Br 9000 Gauss
@Thickness 0.356 mm
heat treatment unknown; ASTM A596
 9000 Gauss
@Thickness 0.635 - 3.17 mm
heat treatment unknown; ASTM A596
Curie Temperature 450 - 500 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.60 µin/in-°F
@Temperature 25.0 - 204 °C
Specific Heat Capacity 0.120 BTU/lb-°F
Thermal Conductivity 13.0 W/m-K
Melting Point 2600 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Iron, Fe >= 51 %As Balance
Manganese, Mn <= 0.50 %
Nickel, Ni <= 48 %
Silicon, Si <= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn
Aperam Mumetal Cold Rolled Strip
Aperam Permimphy Cold Rolled Strip
Aperam Supera 50/50sp Cold Rolled Strip
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality

NHIGH003 / 17306

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.