MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Pibiflex® 4054 IM NERO Copolyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Injection Molding Thermoplastic Copolyester Elastomer

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 41ASTM D2240
Tensile Strength 33.0 MPaASTM D638
Elongation at Break 600 %ASTM D638
Flexural Modulus 90.0 MPaASTM D790
Izod Impact, Notched NB
@Temperature 23.0 °C
ASTM D256/A
 NB
@Temperature -30.0 °C
ASTM D256/A
Tear Strength 98.0 kN/mASTM D624
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 °CASTM D3417
Vicat Softening Point 155 °C120°C/h at 10 N; ASTM D648
Oxygen Index 20 %ASTM D2863
 
Descriptive Properties
Fatigue Resistance (mm/1000 cycles).1/300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® HTR237BG BK320 TPC-ET
Celanese SO.F.TER Laprene® 8K1.A55 TPE
Celanese SO.F.TER Laprene® 83FM.A90 TPE
Celanese SO.F.TER Laprene® 83FM.A30 TPE
Celanese SO.F.TER Laprene® 830.971 TPE

PSOFS777 / 162241

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.