MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Polyetherimide, General Purpose, 5% PTFE, Flame Retardant

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Moisture Absorption at Equilibrium 0.60 %50% RH; ASTM D570
Water Absorption at Saturation 1.1 %
@Temperature 22.8 °C
ISO 62
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 5.0 - 30 g/10 min
@Load 6.70 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 110ASTM D785
Tensile Strength at Break 15000 psiASTM D638
Tensile Strength, Yield 15000 psiASTM D638
Elongation at Break 40 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Tensile Modulus 500000 psiASTM D638
Flexural Strength 21000 psiASTM D790
Flexural Modulus 470 ksiASTM D790
Izod Impact, Notched 1.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 1.00 ft-lb/in
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 10.0 ft-lb/in
@Temperature 22.8 °C
ASTM D4812
Izod Impact, Notched (ISO) 3.50 ft-lb/in²
@Temperature -30.0 °C
ISO 180/1A
 4.20 ft-lb/in²
@Temperature 22.8 °C
ISO 180/1A
Charpy Impact, Notched 5.00 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
Gardner Impact 20.0 in-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 22.0 µin/in-°F
@Temperature -20.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 22.0 µin/in-°F
@Temperature -20.0 - 150 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 400 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 385 °FASTM D648
Vicat Softening Point 409 °FISO 306/B120
 418 °FISO 306/B50
 425 °F120°C/h, 50 N; ASTM D1525
Flammability, UL94 V-0
@Thickness 1.59 mm
 V-0
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 630 - 750 °F
Middle Barrel Temperature 640 - 750 °F
Front Barrel Temperature 650 - 750 °F
Melt Temperature 640 - 750 °F
Mold Temperature 225 - 350 °F
Drying Temperature 290 - 300 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.00100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oxford Polymers 20GF 20% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding
Oxford Polymers 10GF 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding
Oxford Polymers PEI 10GF-Natural PEI, 10% Glass Fiber Reinforced
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced

PPOLYQ200 / 160721

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.