MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound UF0067W Polyphthalamide (PPA)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: LNP THERMOCOMP UF0067W compound is based on Polyphthalamide (PPA) resin containing 30% glass fiber. Added features of this grade include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flame Retardant.

Features: High Stiffness,Flame Retardant,Non-Chlorinated,Non-Brominated,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ASTM D792
 1.45 g/cc0.0524 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/in24hrs; ASTM D955
 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.012 - 0.015 cm/cm0.012 - 0.015 in/in24hrs; ASTM D955
 0.012 - 0.015 cm/cm0.012 - 0.015 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 128 MPa18600 psi5 mm/min; ISO 527
 143 MPa20700 psi5 mm/min; ASTM D638
Elongation at Break 1.9 %1.9 %5 mm/min; ISO 527
 2.5 %2.5 %5 mm/min; ASTM D638
Tensile Modulus 10.54 GPa1529 ksi5 mm/min; ASTM D638
 11.31 GPa1640 ksi1 mm/min; ISO 527
Flexural Strength 189 MPa27400 psiISO 178
 213 MPa30900 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.13 GPa1320 ksi2 mm/min; ISO 178
 10.2 GPa1480 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 64.0 J47.2 ft-lbASTM D256
Izod Impact, Unnotched 6.62 J/cm12.4 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 32.0 kJ/m²15.2 ft-lb/in²80*10*4; ISO 180/1U
Impact Test 1.00 J0.738 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.82
@Frequency 1e+6 Hz
3.82
@Frequency 1e+6 Hz
ASTM D150
 4.05
@Frequency 1000 Hz
4.05
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 29.7 kV/mm
@Thickness 0.800 mm
754 kV/in
@Thickness 0.0315 in
in oil; ASTM D149
Dissipation Factor  0.0115
@Frequency 1000 Hz
0.0115
@Frequency 1000 Hz
ASTM D150
 0.0128
@Frequency 1e+6 Hz
0.0128
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index >= 600 V>= 600 VUL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  23.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 25.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  50.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
28.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 51.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
28.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 299 °C
@Thickness 3.20 mm
570 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 277 °C531 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 281 °C
@Thickness 3.20 mm
538 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 125 °C257 °FUL 746B
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746B
UL RTI, Mechanical without Impact 125 °C257 °FUL 746B
Flammability, UL94  V-1
@Thickness >=1.00 mm
V-1
@Thickness >=0.0394 in
UL 94
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 320 °C536 - 608 °F
Zone 2 280 - 320 °C536 - 608 °F
Zone 3 280 - 320 °C536 - 608 °F
Melt Temperature 280 - 320 °C536 - 608 °FInjection Molding
Mold Temperature 90.0 - 120 °C194 - 248 °F
Drying Temperature 90.0 - 110 °C194 - 230 °FInjection Molding
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hourInjection Molding
Back Pressure 1.00 - 5.00 MPa145 - 725 psi
Screw Speed 30 - 100 rpm30 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81926 / 289873

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.