MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

SABIC XYLEX™ HX8300HP PC+Polyester (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO sterilizable.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.17 g/cc0.0423 lb/in³ISO 1183
Water Absorption 0.49 %0.49 %23°C/sat; ISO 62
Moisture Absorption 0.150 %0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  15 g/10 min
@Load 2.16 kg,
Temperature 265 °C
15 g/10 min
@Load 4.76 lb,
Temperature 509 °F
ASTM D1238
 15 g/10 min
@Load 2.16 kg,
Temperature 265 °C
15 g/10 min
@Load 4.76 lb,
Temperature 509 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 737310s; ASTM D2240
Tensile Strength at Break 46.0 MPa6670 psi50 mm/min; ASTM D638
 54.0 MPa7830 psi50 mm/min; ISO 527
Tensile Strength, Yield 47.0 MPa6820 psi50 mm/min; ASTM D638
 55.0 MPa7980 psi50 mm/min; ISO 527
Elongation at Break 150 %150 %50 mm/min; ASTM D638
 >= 200 %>= 200 %50mm/min; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
 5.0 %5.0 %50 mm/min; ASTM D638
Tensile Modulus 1.52 GPa220 ksi50 mm/min; ASTM D638
 1.60 GPa232 ksi1mm/min; ISO 527
Flexural Strength 78.0 MPa11300 psi2 mm/min; break; ISO 178
Flexural Yield Strength 71.0 MPa10300 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.68 GPa244 ksi1.3 mm/min, 50 mm span; ASTM D790
 1.70 GPa247 ksi2 mm/min; ISO 178
Izod Impact, Notched 11.2 J/cm21.0 ft-lb/inASTM D256
 0.0500 J/cm
@Temperature -30.0 °C
0.0937 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) <= 1.00 kJ/m²<= 0.476 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -10.0 °C
2.38 ft-lb/in²
@Temperature 14.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 7.00 J/cm²33.3 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 95.0 J70.1 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Comparative Tracking Index >= 600 V>= 600 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 85.0 °C185 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C
@Thickness 3.20 mm
174 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °F1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 75.0 °C
@Thickness 3.20 mm
167 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 92.0 °C198 °FRate B/50; ISO 306
 96.0 °C205 °FRate B/50; ASTM D1525
 96.0 °C205 °FRate B/120; ISO 306
Glow Wire Test 750 °C
@Thickness 1.00 mm
1380 °F
@Thickness 0.0394 in
IEC 60695-2-12
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5391.539ISO 489
Haze <= 2.0 %
@Thickness 2.54 mm
<= 2.0 %
@Thickness 0.100 in
ASTM D1003
Transmission, Visible 88 %
@Thickness 2.54 mm
88 %
@Thickness 0.100 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 265 °C473 - 509 °FInjection Molding
Zone 1 240 - 250 °C464 - 482 °F
Zone 2 240 - 260 °C464 - 500 °F
Zone 3 245 - 265 °C473 - 509 °F
Melt Temperature 245 - 265 °C473 - 509 °F
Mold Temperature 45.0 - 60.0 °C113 - 140 °F
Drying Temperature 65.0 - 75.0 °C149 - 167 °FInjection Molding
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %
Back Pressure 0.200 - 0.500 MPa29.0 - 72.5 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00130 - 0.00200 cm0.000512 - 0.000787 in
Screw Speed 20 - 100 rpm20 - 100 rpm
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11625 / 245092

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.