MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Specialty Materials Hy-Bor 100 Boron/Graphite Hybrid Prepreg Tape
Categories: Polymer; Thermoset; Epoxy

Material Notes: Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil boron fibers, Hy-Bor material can be manufactured to incorporate any commercially available graphite prepreg. By altering the spacing of the boron fiber in the prepreg, performance properties and material costs can be tailored to meet the needs of a variety of demanding applications.

Property data reported for 100 filaments/inch 4-mil boron fiber with MR-40 carbon fiber and NCT-301 resin system.

Information provided by Specialty Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.82 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1620 MPa
Elongation at Yield 0.80 %
Modulus of Elasticity 207 GPa
Flexural Yield Strength 2280 MPa
Flexural Modulus 207 GPa
Compressive Yield Strength 2340 MPa
Compressive Modulus 193 GPa
Shear Strength 103 MPaInterlaminar
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 121 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Reaction-Bonded, SiSiC
Schunk CarSIK CT Silicon Carbide
Mullite, 3Al2O3-2SiO2
Goodfellow Carbon/Vinyl Ester Tube
Goodfellow Carbon/Epoxy Composite Rod

PSPEC03 / 68532

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.