MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Taktene® Latex S62 F
Categories: Other Engineering Material

Material Notes: Taktene® Latex S62 is an aqueous dispersion with high content of solids of a butadiene-styrene copolymer produced by cold emulsion polymerization, using a fatty soap as an emulsifier. It has approximately 24% of bound styrene in the copolymer.

CAS No: 9003-55-8

Use: Taktene Latex S62 is used in the production of gel and non-gel laminated foam, molded foam, lining impregnation, carpet backing, agglomerates of coconut fiber and cork, manufacture of insoles, production of chewing gum base, water base adhesives compositions and in modification of asphalt emulsions.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 68 %ASTM D1417
pH 11ASTM D1417
Brookfield Viscosity 800 cPRVT, spindle2, 20 rpm; ASTM D1417
Mooney Viscosity 135ASTM D1646
 
Chemical PropertiesOriginal ValueComments
Styrene Content 24 %Bound; ASTM D5775
 
Processing PropertiesOriginal ValueComments
Shelf Life 4.00 Month
@Temperature 10.0 - 30.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Synthos Latex DL 2256LA Carboxylated SB
Nitriflex Nitrilatex NTL-218 Carboxylated Styrene Butadiene Latex
LG Chemical Lutex 703 SBR Latex
Lanxess Taktene® Latex S62
Dow Latex LXC 8476NA Carboxylated Styrene-Butadiene Latex

PLANY9071 / 209462

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.