MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam 2290 is a self-emulsifying APEO-free organic antifoam concentrate. The product is absolute free of silicone and does not contain any silica.

Application: TEGO® Antifoam 2290 destroys foam or prevents foam formation reliably in aqueous media and may be used for foam control in a variety of industrial applications, even there where the use of silicone and silica is not accepted:

  • process aid for water-based polymerization of dispersions, thermoplastics and elastomers (e. g. demonomerisation of SBR or NBR emulsions, handling of acrylates)
  • in formulation and application of polymer dispersions/latices (e. g. adhesives based on acrylates or PVAc, paper coatings or others)
  • in a multitude of other industrial applications
Properties / Benefits: Due to the special selection of active ingredients TEGO® Antifoam 2290 outperforms conventional organic antifoams.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.860 g/cc
Viscosity 50 - 200 cPdynamic
 
Descriptive Properties
Appearanceyellowish
Content100%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5852 Additive
Evonik TEGOPREN® 5885 Additive
Evonik TEGO® Antifoam 2291 Antifoam concentrate
Evonik TEGOPREN® 5847 Additive
Evonik TEGOPREN® 5851 Defoamer

PEVONIL545 / 196749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.