MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polytek Poly-Optic® 1420 Rigid Clear Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: A versatile, clear polyurethane. A matte finish will give a frosted appearance, and a higher gloss will increase its transparency.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Brookfield Viscosity 250 cP250 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Tensile Strength 54.5 MPa7900 psiPost cured for 16 hours at 160°F
Elongation at Break 5.3 %5.3 %Post cured for 16 hours at 160°F
Modulus of Elasticity 1.182 GPa171.5 ksiPost cured for 16 hours at 160°F
Flexural Strength 86.9 MPa
@Strain 5.0 %
12600 psi
@Strain 5.0 %
Post cured for 16 hours at 160°F
Flexural Modulus 1.72 GPa250 ksiPost cured for 16 hours at 160°F
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.6 °C168 °FPost cured for 16 hours at 160°F
 
Processing PropertiesMetricEnglishComments
Pot Life 15.0 min15.0 min
 
Descriptive Properties
Color / AppearanceWater clearPart A
 Water clearPart B
Demold Time (hrs)0.5@ 175°F
 8@ 150°F
Max Exotherm (°F)3111-lb mass
Mix Ratio by weight2 to 1Part A to Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYT9911 / 287691

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.