MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUMILOY GP2200 Injection Molding Grade, General Purpose 20% Glass Reinforced PPE
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 20% Glass Filled

Material Notes: NSF Certified for KA02 and E2035. Noted for High Flow, High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water contact.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccASTM D792
Melt Flow 9.5 g/10 min
@Load 5.00 kg,
Temperature 280 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 970 kg(f)/cm²
@Thickness 3.20 mm
ASTM D638
Elongation at Break 7.0 %
@Thickness 3.17 mm
ASTM D638
Flexural Strength 137 MPa
@Thickness 3.20 mm
ASTM D790
Flexural Modulus 50000 kg(f)/cm²
@Thickness 3.20 mm
ASTM D790
Izod Impact, Notched 10.5 kg-cm/cm
@Thickness 3.20 mm
ASTM D256
Izod Impact, Unnotched 46.0 kg-cm/cm
@Thickness 3.20 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
@Thickness 3.20 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 300 °C
Middle Barrel Temperature 270 - 310 °C
Front Barrel Temperature 270 - 310 °C
Nozzle Temperature 270 - 310 °C
Mold Temperature 70.0 - 110 °C
Drying Temperature 80 - 100 °C
Dry Time 4 - 5 hour
Moisture Content >= 0.03 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Iupiace® GX1050 m-Polyphenylene Ether (m-PPE)
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE
Mitsubishi Iupiace® GX1210 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® AP6GM2 m-Polyphenylene Ether (m-PPE)
BASF Luranyl® KR 2420 Polyphenylene Ether + Styrene-Butadiene Blend

PLGCHEM255 / 146085

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.