MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) 5030UA High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: HD-5030UA is a high-density polyethylene copolymer grade with a narrow molecular weight distribution, specially developed for injection molding application requiring very high environmental stress cracking resistance.

Applications: caps & closures for the packaging of sparkling water and carbonated soft drinks, technical parts.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D1505
Environmental Stress Crack Resistance 30 hourASTM D1894
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 27.0 MPaASTM D638
Elongation at Break 1000 %ASTM D638
Flexural Modulus 1100 MPaASTM D790
Charpy Impact, Notched 15.0 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 123 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 130 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene
Dow DOWLEX™ IP-10 High Density Polyethylene
Iran Petrochemical (PCC) 5218EA High Density Polyethylene
Iran Petrochemical (PCC) 52511 High Density Polyethylene

PIPC226 / 149688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.