Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC VALOX™ VX3101N PBT (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.31
g/cc
ISO 1183
Water Absorption
0.34 %
23°C/sat; ISO 62
Moisture Absorption
0.0800 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.011
-
0.018
cm/cm
SABIC method
Linear Mold Shrinkage, Transverse
0.0090
-
0.018
cm/cm
SABIC method
Melt Flow
20
g/10 min
@Load 1.20 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
100
MPa
ISO 2039-1
Tensile Strength at Break
50.0
MPa
50 mm/min; ISO 527
Tensile Strength, Yield
65.0
MPa
50 mm/min; ISO 527
Elongation at Break
15 %
50 mm/min; ISO 527
Elongation at Yield
3.5 %
50 mm/min; ISO 527
Tensile Modulus
2800
MPa
1mm/min; ISO 527
Flexural Yield Strength
85.0
MPa
2 mm/min; ISO 178
Flexural Modulus
2600
MPa
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
4.00
kJ/m²
80*10*4; ISO 180/1A
2.00
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
2.00
kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
NB
80*10*4; ISO 180/1U
NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched
NB
Edgew 80*10*4 sp=62mm; ISO 179/1eU
NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
5.00
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
3.00
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles
9.0
CS-17, 1 kg; SABIC method
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+15
ohm
ROA; IEC 60093
Dielectric Constant
2.9
@Frequency 1e+6 Hz
IEC 60250
3.1
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength
16.0
kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor
0.0020
@Frequency 50.0 - 60.0 Hz
IEC 60250
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
600
V
IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
130
µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
130
µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Hot Ball Pressure Test
125
°C
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
175
°C
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)
60.0
°C
1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point
183
°C
Rate B/50; ISO 306
185
°C
Rate B/120; ISO 306
Flammability, UL94
HB
@Thickness 1.50 mm
UL 94 by SABIC-IP
Oxygen Index
20 %
ISO 4589
Glow Wire Test
850
°C
@Thickness 1.00 mm
IEC 60695-2-12
Processing Properties
Original Value
Comments
Processing Temperature
40.0
-
60.0
°C
Hopper Temperature
Nozzle Temperature
240
-
260
°C
Injection Molding
Zone 1
230
-
245
°C
Zone 2
240
-
255
°C
Zone 3
245
-
265
°C
Melt Temperature
250
-
270
°C
Mold Temperature
40.0
-
100
°C
Drying Temperature
110
-
120
°C
Injection Molding
Dry Time
2.00
-
4.00
hour
Injection Molding
Moisture Content
0.020 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABI10307 / 243774
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.