MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 20%Glass Fiber Filled

Material Notes: Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resistance of the material, while maintaining most of its other basic characteristics. The combination of structural properties and cost effectiveness make this resin an attractive alternative to metals in many engineering applications. Veradel® 3320GF is an opaque, grayish material in its natural form and can be readily colored.

This grade was formerly marketed as Gafone™ PESU.

Key Attributes: Acid Resistant; Creep Resistant; Flame Retardant; Good Adhesion; Good Dimensional Stability; High Rigidity; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight

Applications: Metal Replacement

1. These properties has been determined from injection molded test specimen under ideal processing parameters and conditioned at 23+/- 2°C and 50%RH.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ASTM D792
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inASTM D255
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 120 MPa17400 psiASTM D638
Elongation at Break 2.8 %2.8 %ASTM D638
Tensile Modulus 7.00 GPa1020 ksiASTM D638
Flexural Strength 170 MPa24700 psiASTM D790
Flexural Modulus 6.50 GPa943 ksiASTM D790
Izod Impact, Notched 0.700 J/cm1.31 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+14 ohm1.00e+14 ohmASTM D257
Dielectric Strength 20.0 kV/mm508 kV/inASTM D149
Arc Resistance 110 sec110 secASTM D495
Comparative Tracking Index 150 V150 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FASTM D696
Maximum Service Temperature, Air 190 °C374 °FContinuous; ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FAnnealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
UL 94
Oxygen Index 42 %42 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Die Temperature 300 - 320 °C572 - 608 °FExtrusion
Melt Temperature 340 - 380 °C644 - 716 °F
Mold Temperature 120 - 160 °C248 - 320 °F
Drying Temperature 150 °C
@Time 10800 sec
302 °F
@Time 3.00 hour
Screw Speed 20 - 50 rpm20 - 50 rpm
 
Descriptive Properties
Availability (as of March 2019)Africa & Middle East; Asia Pacific; Europe; Latin America; North America
ColorColors Available; Opaque
FormsPellets
ProcessingInjection Molding
RoHS ComplianceRoHS Compliant

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Veradel® AG-230 Polyethersulfone
Syensqo (Solvay Specialty Polymers) Veradel® 3300 Polyethersulfone (PESU)
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer
BASF Ultrason® E 6020 P PES
BASF Ultrason® E 2010 G6 30% Glass Filled PES

PSOL8Y5465 / 238846

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.