MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
JSC Agidol-12? Antioxidant for Biodiesel
Categories: Other Engineering Material

Material Notes: Description: ?gidol-12? is a mixture of alkylphenols perfectly calibrated in order to obtain the best synergy between the components and to enhance the antioxidant properties. This product is used as an antioxidant additive to biodiesel fuel to enhance chemical stability.

Information provided by JSC, Synthez-Kauchuk

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 0.910 g/ccASTM D1298
Viscosity Measurement <= 6.0[mm2/s]; ASTM D 445
 
Thermal PropertiesOriginal ValueComments
Crystallization Temperature <= 65.0 °CASTM D 1177
Flash Point <= 60.0 °Cclosed cup; ASTM D 92
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %ASTM D 95
 
Descriptive Properties
Appearancemolten mass from light to dark yellow in color
Content1Mass fraction of the active ingredient
Mass fraction<20%4,6-di-tert-butyl-o-cresol
 <20%2,6-di-tert-butylphenol
 >50%2,6-di-tert-butyl-p-cresol
Oxidation stability>6110°C and dosage of 0.25% wt. per hour, ASTM D 2274

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSC007 / 317827

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.