Description Solvent-containing adhesive based on Polychloroprene rubber which exhibits good sprayability and excellent heat resistance. Properties: swift®col 2411 is suitable for bonding rubber, foamed plastics, textile, microcelular rubber, metal foil, insulation material, etc., to primed and lacquered sheet, metal, wood fiber board. Especially suitable for applications in Automotive Industry, i.e. bonding of preformed headliners, and on the whole, when high heat resistance is required. Due to its formulation, swift®col 2411 performs good adhesion on materials with low surface tension, such as EPDM, PP, etc. Preliminary tests are necessary on each particular application. Information provided by H.B. Fuller Company |