MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Unifrax Fiberfrax® Duraboard® LD Ceramic Fiber Board
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard products offer low thermal conductivity, high temperature stability, uniform density, and excellent resistance to thermal shock and chemical attack.

This product possesses the same density and temperature rating as Duraboard RG insulation, but is manufactured to tighter dimensional tolerances and has an excellent finished surface. These characteristics make it ideally suited for use as a sandwich or core material or for use in the manufacture of components where aesthetic quality, as well as uniformity and performance, is important.

Description: A higher quality surface finish with tighter dimensional tolerances make this board suitable for use in situations where aesthetic quality, as well as performance, is important.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 16.0 lb/ft³Nominal
Loss On Ignition 6.0 - 7.0 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0800 ksiFired (24 hrs at cont. use)
 0.200 ksiGreen (typ.)
Compressive Strength 22.0 psi10% Deformation; Fired
 23.0 psi5% Deformation; Fired
 23.0 psi15% Deformation; Fired
 42.0 psi5% Deformation; Green
 50.0 psi10% Deformation; Green
 57.0 psi15% Deformation; Green
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 27.0 V/mil
 
Thermal PropertiesOriginal ValueComments
Melting Point 1760 °C
Maximum Service Temperature, Air 1149 °CRecommended Operating Temperature
Shrinkage <= 5.0 %
@Time 86400 sec
at Recommended Operating Temperature
 
Descriptive Properties
ColorCream / white
Fiberfrax® Fibers (%)100
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
NeoGraf eGRAF® HITHERM™ HT-1220 Graphite
Unifrax Fiberfrax® 880 Ceramic Fiber Paper

CUNIF027 / 97799

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.