MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
P & P Technology EC-S Pure Silver Loaded Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: P & P Technology material reference EC-S is a silicone elastomer with Silver conductive filler. It is tan in color. The material is specially compounded to offer excellent physical and electrical properties over an effective temperature range of –50 to + 150°C. Silicone offers excellent performance over a wide temperature range with good resistance to chemicals and weathering. Its resistance to mineral based fluids is limited, but it has good splash contact resistance to most mineral oils and greases.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1.25 MPaASTM D412
Elongation at Break >= 100 %ASTM D412
Tear Strength >= 8.75 kN/m
Compression Set <= 30 %
@Temperature 100 °C,
Time 259000 sec
ASTM D395
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.0020 ohm-cmMil-G-83528
Shielding Effectiveness 70 dB
@Frequency 200000 Hz
Mil-G-83528/Mil std 285
 115 dB
@Frequency 1e+8 Hz
Mil-G-83528/Mil std 285
 115 dB
@Frequency 5.00e+8 Hz
Mil-G-83528/Mil std 285
 115 dB
@Frequency 2.00e+9 Hz
Mil-G-83528/Mil std 285
 115 dB
@Frequency 1e+10 Hz
Mil-G-83528/Mil std 285
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
NuSil EPM-2463 Silicone, Thermal Interface Material (TIM): Electrically Conductive
NuSil R-2634 Silicone, Electrically Conductive
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer
Parker Chomerics CHO-FORM 5531 EMI Shielding Material

PPPTEC024 / 133488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.