MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Hilox ™ 880 Mac-A860S Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: An alumina ceramic of 86% Al2O3 content, that combines mechanical strength with excellent electrical properties.

Prime Features:

  • Excellent electrical insulator at high temperatures
  • Good dimensional stability
  • High mechanical strength
  • Good abrasion resistance
  • Non-porous and vacuum tight
  • Corrosion resistant
Typical Applications:
  • Components in domestic appliances, especially where parts handling and assembly operations are automated
  • Thermostat assembles for electric irons, kettles and fires
  • Immersion heaters
  • End bushes for sheathed heating elements
  • Thermocouples
  • Cartridge heaters
Production Capabilities:
  • Complex components custom-manufactured to close tolerances
  • Prototype, batch and volume production
  • Comprehensive range of bushes, rings, rods and tubes for high temperature electrical insulators.

Information provided by Morgan Advanced Materials

Key Words: Mac-A860S
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.54 g/cc0.128 lb/in³fired
Open Porosity 0.00 %0.00 %fully dense, % nominal, apparent
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell HR45N 77.177.1
Modulus of Elasticity 250 GPa
@Temperature 20.0 °C
36300 ksi
@Temperature 68.0 °F
Flexural Strength 353 MPa
@Temperature 20.0 °C
51200 psi
@Temperature 68.0 °F
3-point
Compressive Strength 1800 MPa261000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 1.00e+6 ohm-cm
@Temperature 600 °C
>= 1.00e+6 ohm-cm
@Temperature 1110 °F
 >= 1.00e+8 ohm-cm
@Temperature 300 °C
>= 1.00e+8 ohm-cm
@Temperature 572 °F
 >= 1.00e+14 ohm-cm
@Temperature 20.0 °C
>= 1.00e+14 ohm-cm
@Temperature 68.0 °F
Dielectric Constant 8.5
@Frequency 1e+6 Hz
8.5
@Frequency 1e+6 Hz
Dielectric Strength 28.0 kV/mm711 kV/in
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.20 µm/m-°C
@Temperature 20.0 - 1000 °C
4.56 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.920 J/g-°C0.220 BTU/lb-°F
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 °C
104 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1200 °C2190 °Fno load
 
Component Elements PropertiesMetricEnglishComments
Al2O3 86 %86 %
 
Descriptive Properties
Colorwhite
Thermal Downshock180 sC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Hilox™ 880 84-86% Alumina
85% Alumina, vitreous body

CMORF5016 / 200254

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.