MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound RF0049S Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP THERMOCOMP RF0049S compound is based on Nylon 6/6 resin containing 20% glass fiber. Added features of this grade include: Flame Retardant, Heat Stabilized.

Features: High Stiffness,Flame Retardant,Heat Stabilized,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³ASTM D792
Moisture Absorption 0.150 - 0.250 %0.150 - 0.250 %Injection Molding
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm0.010 - 0.012 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 136 MPa19700 psiASTM D638
Elongation at Break 3.3 %3.3 %ASTM D638
Flexural Strength 199 MPa28900 psiASTM D790
Flexural Modulus 7.51 GPa1090 ksiASTM D790
Izod Impact Notched 85.0 J62.7 ft-lbASTM D256
Izod Impact, Unnotched 6.78 J/cm12.7 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI  60 - 120 sec
@Thickness >=1.70 mm
60 - 120 sec
@Thickness >=0.0669 in
UL 746A
 >= 120 sec
@Thickness >=3.00 mm
>= 120 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness >=1.70 mm
60 - 120 arcs
@Thickness >=0.0669 in
UL 746A
 >= 120 arcs
@Thickness >=3.00 mm
>= 120 arcs
@Thickness >=0.118 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 105 °C221 °FUL 746B
UL RTI, Mechanical without Impact 115 °C239 °FUL 746B
Flammability, UL94 V-0
@Thickness >=1.70 mm
V-0
@Thickness >=0.0669 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 280 - 295 °C536 - 563 °F
Zone 3 295 - 305 °C563 - 581 °F
Melt Temperature 275 - 290 °C527 - 554 °FInjection Molding
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81848 / 289795

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.