MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake EC471 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Excellent processability, very low neck-in, excellent heat sealability, very good draw down and good moisture barrier.

    Application/Uses
  • Laminations
  • Food packaging
  • High speed coatings
  • Low coat weights
  • General purpose coatings

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Excellent processability, very low neck-in, excellent heat sealability, very good draw down and good moisture barrier
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Melt Flow 10 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1400 psiASTM D638
Elongation at Break 450 %ASTM D638
 
Processing PropertiesOriginal ValueComments
Melt Temperature 575 - 625 °F
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman 1840A Polyethylene
Bamberger Polymers Bapolene® 1030 Low Density Polyethylene Extrusion/Injection Resin
Armacell OleTex® BKJN 200 LDPE Foam
Armacell OleTex® BCJN 200 EVA/LDPE Foam
Aclo Accucomp Polyethylene LD0109L Low Density

PWESF033 / 84470

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.