HD5030EA is high density polyethylene copolymer containing butene-1(C4) as comonomer. HD5030EA has good impact strength, excellent surface finish. This grade has food contact approval. Applications: caps and closures for packaging.Information provided by Tabriz Petrochemical Company. |