MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil NTX™ NTX 101 Super Strength Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copolymers. It is stabilized for blown film extrusion and does not contain slip or antiblock, making it well suited for blown stretch wrap.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/ccASTM D1505
Thickness 1.00 mil
Melt Flow 0.90 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1320 psiat 2% offset; ASTM D882
Film Tensile Strength at Yield, TD 1360 psiat 2% offset; ASTM D882
Film Elongation at Break, MD 630 %ASTM D882
Film Elongation at Break, TD 720 %ASTM D882
Puncture Energy 32.0 in-lbExxonMobil
Elmendorf Tear Strength, MD 460 g/milASTM D1922
Elmendorf Tear Strength, TD 600 g/milASTM D1922
Dart Drop 330 g/milASTM D1709
Film Tensile Strength at Break, MD 9080 psiASTM D882
Film Tensile Strength at Break, TD 7370 psiASTM D882
1% Secant Modulus, MD 23700 psiASTM D882
1% Secant Modulus, TD 26500 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 253 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 109 °CExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 17 %ASTM D1003
Gloss 37 %45°; ASTM D2457
 
Descriptive Properties
FeaturesThermal Stabilizer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil NTX™ NTX 095 Super Strength Film Resin
ExxonMobil NTX™ NTX 104 Super Strength Film Resin
ExxonMobil NTX™ NTX 150 Super Strength Film Resin
ExxonMobil NTX™ NTX 141 Super Strength Film Resin
ExxonMobil LL 3201.36 Premium High Strength Film Resin

PEXB244 / 37549

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.