MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BRP Manufacturing AA615 Premium SBR Rubber Sheet
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Material: Premium SBR Rubber Sheet
BRP Style: AA615
Finish: Smooth (Fabric Finish is Available)
ASTM Callout: ASTM D2000 4AA615A13B13C12EA14F17G21

Information provided by BRP Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 1450 psiOriginal; ASTM D412
 <= 1087.5 psi
@Temperature 70.0 °C,
Time 252000 sec
A13 – Heat Resistance; ASTM D573
 1015 - 1885 psi
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged; ASTM D573
Elongation at Break 350 %Original; ASTM D412
 <= 175 %
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged; ASTM D573
 <= 262.5 %
@Temperature 70.0 °C,
Time 252000 sec
A13 – Heat Resistance; ASTM D573
Compression Set <= 25 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395 Method B
 <= 50 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 212 °F
Minimum Service Temperature, Air -40.0 °F
 
Descriptive Properties
Hardness45-75Heat Aged, ASTM D573, 70 h @ 70°C
 55-65ASTM D2240
 70A13 – Heat Resistance, ASTM D573, 70 hours @ 70°C
Resistance to Ozone>100%C12, ASTM D1171

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBRPM064 / 315725

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.