MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Glass Fiber Filled

Material Notes: AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength and stiffness than unfilled AV-650 resin. This material can be repeatedly exposed to harsh chemicals and prolonged steam sterilization cycles without any significant loss of properties. Potential applications for this resin include orthopedic and dental instruments, surgical power tool battery housings and other devices and components requiring a combination of high temperature performance and high environmental resistance. AvaSpire® AV-650 GF30 can be easily processed by typical injection molding and extrusion methods using standard equipment.

Features: Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Strength

Uses: Medical/Healthcare Applications; Oil/Gas Applications; Power/Other Tools

Additional Properties: Water Absorption - ASTM D570 0.40 %

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccASTM D792
Filler Content 30 %Glass Fiber
Water Absorption 0.20 %
@Time 86400 sec
ISO 62
Viscosity 410000 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt Viscosity; ASTM D3835
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.18 mm
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 in/in
@Thickness 3.18 mm
ASTM D955
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100ASTM D785
Tensile Strength 142 MPaASTM D638
Tensile Strength, Yield 165 MPa5 mm/min, Type 1A; ISO 527-2
Elongation at Break 2.6 %Type 1A, 5 mm/min; ISO 527-2
 2.6 %5 mm/min; ASTM D638
Tensile Modulus 10100 MPaASTM D638
 10500 MPaISO 527-2
Flexural Strength 221 MPaASTM D790
 240 MPaISO 178
Flexural Modulus 9000 MPaASTM D790
 9800 MPaISO 178
Compressive Strength 163 MPaASTM D695
Shear Strength 80.8 MPaASTM D732
Izod Impact, Notched 96.0 J/mASTM D256
Izod Impact, Unnotched 960 J/mASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 69.0 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.6
@Frequency 1e+6 Hz
ASTM D150
 3.65
@Frequency 60 Hz
ASTM D150
 3.66
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 14.0 kV/mm
@Thickness 3.18 mm
ASTM D149
Dissipation Factor 0.0020
@Frequency 60 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
Specific Heat Capacity 1.29 J/g-°C
@Temperature 50.0 °C
ASTM C351
 1.67 J/g-°C
@Temperature 200 °C
ASTM C351
Thermal Conductivity 0.290 W/m-KASTM C177
Melting Point 340 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 209 °C
@Thickness 3.20 mm
Annealed; ASTM D648
Glass Transition Temp, Tg 158 °CDSC
Flammability, UL94 V-0
@Thickness 0.800 - 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 365 °C
Middle Barrel Temperature 370 °C
Front Barrel Temperature 375 °C
Nozzle Temperature 380 °C
Melt Temperature 365 - 390 °C
Mold Temperature 150 - 180 °C
Drying Temperature 150 °C
@Time 14400 sec
 
Descriptive Properties
Agency RatingsFAA FAR 25.853a
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorBeige
FormPellets
Injection RateFast
Processing TechniqueInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.0:1.0 to 3.0:1.0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 3805 Polyaryletherketone (PAEK), Glass Fiber 30%
RTP Company RTP 3803 Polyaryletherketone (PAEK), Glass Fiber 20%
Akro-Plastic Akrotek® PEEK GF 30 natural (5047) PEEK, Dry, 30% Glass Filled

PSOL8Y7015 / 176746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.