MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin DAI-EL G-211 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: DAI-EL G-211 is a fluoroelastomer which has excellent adhesion to metal and mechanical properties.

Introduction: DAI-EL G-211 is a diamine type terpolymer of vinylidene fluoride, tetrafluoroethylene and hexafluoropropylene which is suitable for compression molding; It offers excellent adhesion to metal and mechanical properties

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.87 g/cc1.87 g/cc
Mooney Viscosity  23.0
@Temperature 140 °C
23.0
@Temperature 284 °F
ML1+10; ASTM D1646
 47.0
@Temperature 121 °C
47.0
@Temperature 250 °F
ML1+10; ASTM D1646
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78.078.0peak; ASTM D2240
 75.0
@Time 3.00 sec
75.0
@Time 0.000833 hour
ASTM D2240
Tensile Strength 14.7 MPa2130 psiASTM D412
Elongation at Break 240 %240 %ASTM D412
100% Modulus 4.30 MPa
@Strain 100 %
624 psi
@Strain 100 %
ASTM D412
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -15.0 °C5.00 °FLow Temperature Retraction (TR10); ASTM D1329
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 68.5 %68.5 %
 
Descriptive Properties
AppearanceMilky white to pale yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIK9652 / 327092

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.