MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Corr-Paint™ CP2090 High Temperature Epoxy Protective Coating
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Two-part, low viscosity, room temperature curing, epoxy sealer for continuous applications to 400°F (204°C).

Vendors: Aremco offers a wide range of ceramic, epoxy, urethane, and silicone sealers for thermal spray applications from 300°F (150°C) to 3000°F (1650°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Solids Content 100 %100 %Weight
 100 %100 %Volume
Volatiles 0.00 %0.00 %
Viscosity 100 - 200 cP100 - 200 cP
Thickness 1.00 microns0.0394 milWet Film Thickness
 1.00 microns0.0394 milDry Film Thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Flash Point >= 93.3 °C>= 200 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FApplication Temperature
Dry Time >= 1.00 hour>= 1.00 hourCuring, Min Air Set
Cure Time  180 min
@Temperature 65.6 °C
3.00 hour
@Temperature 150 °F
Option B
 2880 min
@Temperature 22.8 °C
48.0 hour
@Temperature 73.0 °F
Option A
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorAmber
Mix Ratio100:25
Theoretical Dry Film Coverage, ft2/gal1604
ThinnerXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAREM961 / 316321

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.