MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Kendall® Special Limited-Slip Gear Lubricant Sea Grade 80W-90
Categories: Fluid; Lubricant

Material Notes: Kendall® Special Limited-Slip Gear Lubricant is an extremepressure, API GL-5, SAE 80W-90 automotive gear oil specially formulated to satisfy the lubrication needs of most limited-slip rear axles. It is friction-modified to help eliminate the stick-slip chatter associated with low-speed, high-torque operation of limited-slip differentials while turning corners with some passenger cars and light trucks. Special Limited-Slip Gear Lubricant is formulated to provide long service life and extended gear life in automotive differentials operating under varying conditions of speed, load, temperature and torque. The carefully balanced formulation is designed to minimize oxidative sludge and varnish formation, reduce wear, prevent scoring damage, and protect against metal fatigue under shock-load conditions.

Applications:

  • Passenger car and truck axles with either conventional or limited-slip differentials
  • Suitable for initial fill of new or rebuilt limited-slip differentials, for top-off, and for refill after a complete drain
Special Limited-Slip Gear Lubricant meets or exceeds the requirements of:
  • API Service GL-5
  • Mack GO-J
  • MIL-PRF-2105E
  • SAE J2360
Features/Benefits:
  • Excellent oxidation resistance and thermal stability to minimize sludge and varnish formation
  • Excellent thermal durability and extreme-pressure properties for extended gear life
  • High load-carrying capacity for protection against scuffing and wear
  • Protects against rust and corrosion
  • Good foam resistance
  • Friction-modified to prevent chatter in limited-slip and positraction differentials

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.891 g/cc0.891 g/cc
Density 0.889 g/cc0.0321 lb/in³
Brookfield Viscosity 90000 cP
@Temperature -26.0 °C
90000 cP
@Temperature -14.8 °F
Viscosity Measurement 102102Index
Kinematic Viscosity at 40°C (104°F) 140 cSt140 cSt
Kinematic Viscosity at 100°C (212°F) 14.5 cSt14.5 cSt
ASTM Color 3.03.0ASTM D1500
 
Thermal PropertiesMetricEnglishComments
Pour Point -30.0 °C-22.0 °F
Flash Point 212 °C414 °FCOC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5311 / 198564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.