MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Avient Edgetek® PF-20GF/000 Polysulfone (PSU)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
Filler Content 20 %Glass Fiber Reinforcement
Water Absorption 0.20 %@ 24 hrs; ASTM D570
Water Absorption at Saturation 0.60 %ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cmASTM D955
 0.0030 - 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 92ASTM D785
Tensile Strength at Break 103 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 5520 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 152 MPaASTM D790
Flexural Modulus 5520 MPaASTM D790
Compressive Strength 138 MPaASTM D695
Shear Strength 62.7 MPaASTM D732
Izod Impact, Notched 69.0 J/m
@Thickness 6.35 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 29.0 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 185 °C
@Thickness 3.18 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 179 °C
@Thickness 3.18 mm
Annealed; ASTM D648
Flammability, UL94 V-0UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 338 - 371 °C
Mold Temperature 93.3 - 149 °C
Drying Temperature 135 °C
Dry Time 2.00 hour
 
Descriptive Properties
FormsPellets
Generic MaterialPSU
Generic NamePolysulfone (PSU)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 South America
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultrason® S 2010 G4 20% Glass Filled PSU
Ensinger TECASON™ S Polysulfone (PSU)
Overview of materials for Polysulfone (PSU)
BASF Ultrason® S 2010 G6 30% Glass Filled PSU
BASF Ultrason® S 2010 PSU

PH0POL0174 / 144743

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.