MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® 18 Corrugated Acrylic Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: When the sun beats down, it stays pleasantly light and cool under roofs glazed with white translucent ACRYLITE® Corrugated acrylic sheet thanks to HEATSTOP, the special IR-(infrared) reflecting surface coating. ACRYLITE Corrugated sheet is extruded from impact-modified acrylic (polymethyl methacrylate, PMMA) to be more break-resistant than sheet made from conventional acrylic, and is guaranteed to be hail-resistant. ACRYLITE Corrugated sheet with HEATSTOP is supplied in a 76/18 profile (length of corrugation / clear height in mm). This product is extremely resistant to weathering and aging, it does not become yellow or brittle, and retains its smooth surface to inhibit dirt from adhering. These properties make corrugated sheet ideally suited for
  • patio roofs
  • carports
  • walkways
  • trellises
  • windscreens
  • roofing

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3000 microns
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 2.20 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µin/in-°F
Maximum Service Temperature, Air 70.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 45 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Acrylite® 8N Acrylic Polymer
Röhm Acrylite Plus® zdf Impact Acrylic Polymer
Röhm Acrylite Plus® zk3HR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4BR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4HR Impact Acrylic Polymer

PEVONIL055 / 196259

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.