MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reltek BONDiT™ B-4682 Adhesive, Sealant & Coating System
Categories: Polymer; Adhesive; Thermoset

Material Notes: Excellent adhesion to low surface energy plastics without primer or surface preparation.

Applications: High flexibility, 300% elongation, emphasizing high tack for un-abraded substrates and plastic films. Excellent for water and oil sealing. Can be applied to oily surfaces. Ambient or thermal cure. May be catalyzed for fast set time.

Key Words: Epoxy Adhesive, Sealant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2350 psi
Elongation at Break 200 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -50.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hour
@Temperature 93.3 °C
 12.0 hour
@Temperature 22.2 °C
 
Descriptive Properties
Chemical & Moisture Resistance1.50=Lowest, 4=Highest

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Armacell Ensolite™ MLC-Black PVC/NBR
Chlorosulfonated Polyethylene Rubber (CM, CSM)
Elantas EN-8 (Conap) Casting, Potting, and Molding Compound
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Polynorbornene Rubber (PNR)

PAQREL08 / 24224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.