MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® RG-17279 BLK 9004 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-17279 BLK 9004 is specifically designed for food contact applications and other regulated markets such as children’s and infants products. Monprene RG-17279 BLK 9004 is a medium density, high hardness grade that is suitable for extrusion and injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; Medium Density; Medium Hardness; Lubricated

Uses: Closures; Consumer Applications; Cookware Handles; Grommets; Handles; Kitchenware; Knobs; Rubber Replacement; Tubing; Toys

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.963 g/ccASTM D792
Viscosity 110 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ISO 11443
Melt Flow 24 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 77
@Time 5.00 sec
ASTM D2240
 79
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1260 psiDie C, 20 in/min, Flow; ASTM D412
Tensile Stress at Strain 499 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 709 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 660 %Die C, 20 in/min, Flow; ASTM D412
Compression Set 30 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 390 - 480 °FMelt, Injection
Rear Barrel Temperature 360 - 450 °FInjection
Middle Barrel Temperature 370 - 460 °FInjection
Front Barrel Temperature 380 - 470 °FInjection
Nozzle Temperature 390 - 480 °FInjection
Zone 1 360 - 450 °FExtrusion
Zone 2 370 - 460 °FExtrusion
Zone 3 380 - 470 °FExtrusion
Zone 4 380 - 470 °FExtrusion
Zone 5 390 - 480 °FExtrusion
Die Temperature 390 - 480 °FExtrusion
Mold Temperature 95.0 - 120 °F
Injection Pressure 200 - 800 psiInjection
Back Pressure 25.0 - 100 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0930 / 237421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.