MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Neostar FN007 Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP

Material Notes: Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copolymer has also found use in tubing and packaging applications. Its excellent chemical, heat, and puncture resistance combined with its strength and durability make it a good choice for applications that require flex-crack resistance and a general utility in harsh environments. Neostar FN007 can be injection molded, extruded in blown film or tubing, or extrusion blow molded. The target inherent viscosity of this product is 1.23.

Applications/Uses

  • Automotive
  • Flexible hinges
  • Pricing channels
  • Retail pricing fins
  • Driver and passenger side air bags
  • Packaging
  • Profiles
  • Tubing
  • Key Attributes

  • Environmentally preferred, non-halogenated material
  • Excellent chemical resistance
  • Exceptional heat resistance and high temperature dimensional stability
  • High flexibility without plasticizers
  • Solvent bondable
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
    Water Absorption 0.40 %0.40 %24h Immersion; ASTM D570
    Viscosity Measurement 1.231.23Inherent; EMN-A-AC-G-V-1
    Melt Flow 4.0 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    4.0 g/10 min
    @Load 4.76 lb,
    Temperature 446 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 9595ASTM D2240
    Hardness, Shore D 5555ASTM D2240
    Tensile Strength at Break 23.0 MPa3340 psiASTM D638
    Tensile Strength, Yield 13.0 MPa1890 psiASTM D638
    Elongation at Break 400 %400 %ASTM D638
    Elongation at Yield 38 %38 %ASTM D638
    Tensile Modulus 0.170 GPa24.7 ksiASTM D638
    Flexural Modulus 0.150 GPa21.8 ksiASTM D790
    Izod Impact, Notched 0.400 J/cm
    @Temperature -40.0 °C
    0.749 ft-lb/in
    @Temperature -40.0 °F
    ASTM D256
    Tear Strength, Total 350 N78.7 lb (f)ASTM D1004
     
    Thermal PropertiesMetricEnglishComments
    Heat of Fusion 27.0 J/g11.6 BTU/lbASTM E793
    CTE, linear 150 µm/m-°C
    @Temperature 20.0 °C
    83.3 µin/in-°F
    @Temperature 68.0 °F
    ASTM D696
    Specific Heat Capacity 1.60 J/g-°C0.382 BTU/lb-°FDSC
     1.80 J/g-°C
    @Temperature 100 °C
    0.430 BTU/lb-°F
    @Temperature 212 °F
    DSC
     2.00 J/g-°C
    @Temperature 150 °C
    0.478 BTU/lb-°F
    @Temperature 302 °F
    DSC
     2.30 J/g-°C
    @Temperature 175 °C
    0.550 BTU/lb-°F
    @Temperature 347 °F
    solid; DSC
     2.30 J/g-°C
    @Temperature 225 °C
    0.550 BTU/lb-°F
    @Temperature 437 °F
    melt; DSC
     3.10 J/g-°C
    @Temperature 200 °C
    0.741 BTU/lb-°F
    @Temperature 392 °F
    transition; DSC
    Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FASTM C177
    Melting Point 205 °C401 °FCrystalline Peak; ASTM D3418
    Crystallization Temperature 140 °C284 °Fon cooling; DSC
    Vicat Softening Point 170 °C338 °F1kg load; ASTM D1525
    Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746
    Glass Transition Temp, Tg -3.00 °C26.6 °FDSC
    Clash Berg Stiffness Temperature <= -70.0 °C<= -94.0 °Fat 930 MPa; ASTM D1043
     -28.0 °C-18.4 °Fat 240 MPa; ASTM D1043

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Eastman Neostar FN005 Elastomer
    Eastman Neostar FN006 Elastomer
    Sorbothane Polyurethane Damping Material, 50 Durometer
    Sorbothane Polyurethane Damping Material, 70 Durometer
    Sorbothane Polyurethane Damping Material, 30 Durometer

    PE9091 / 35147

    Visit Zeus Inc. for PEEK Tubing

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.