MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Spartech Formalloy LG Low-Gloss TPO Alloy Specialty Sheet
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); TPO

Material Notes: Description: Specialty Sheet

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength at Break 3200 psiASTM D638
Elongation at Break 200 %ASTM D638
Flexural Modulus 220000 psiASTM D790
Falling Dart Impact >= 29.16 ft-lb-30°F; ASTM D3029
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 180 °FASTM D648
 
Optical PropertiesOriginal ValueComments
Gloss 35 - 40 %Gardner; ASTM D2523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion
Spartech Formalloy HG High-Gloss TPO Alloy Specialty Sheet
Spartech Formalloy TPR Thermoplastic Rubber Alloy Specialty Sheet
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer
Samyang Triel® 5350 Thermoplastics Polyetherester Elastomer, General Extrusion

PSPAR009 / 68450

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.